MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Bohler-Uddeholm COMPAX™ AISI S7 MOLD QUALITY Cold Work Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Tool Steel; Cold Work Steel

Material Notes: Chromium-molybdenum alloyed steel

A versatile S7 grade recommended for applications demanding a high degree of toughness and moderate wear resistance. Successfully used for heavy-duty punching and shearing tools. Also for hardened back-up plates and punch die holders.

Compax Supreme is characterized by:

  • High toughness
  • Good wear resistance
  • High impact resistance
  • Good through hardening properties
  • Good machinability
  • Excellent polishability
  • Good dimensional stability during hardening
Applications:
MOLDS FOR PLASTICS-Compax Supreme has been developed as a mold quality steel, based on the widely used AISI S-7 grade. The steel is extremely clean and has a homogeneous microstructure. These features are achieved through strict processing control and maximum sulfur content of 0.005%. This quality level is verified by ultrasonic testing to high requirements. The result is a steel that machines consistently, is predictable in heat treatment and can be polished to extremely high surface finishes. Further, the toughness of the steel is enhanced, for greater performance security and increased tool life. By holding the carbon content to the high end of the carbon range a consistent hardness is assured, important in molds with larger cross-sections. Compax Supreme is manufactured in the form of hot rolled and forged bars with a machined, decarbfree finish, with plus tolerances to allow finishing at a nominal inch size, where required.
TOOLS FOR METAL STAMPING-Compax Supreme is also suitable for a wide range of heavy duty blanking, shearing and forming tools, due to its excellent combination of toughness and wear resistance. Its relatively high carbon content makes the achievement of the maximum recommended working hardness of 58 HRC easier to achieve in larger cross sections.
BLANKING AND SHEARING-Tools for: Blanking, punching, cropping, shearing, trimming, Shear blades(cold), Shredding knives, Shear blades(hot, Circular shears, and Trimming Tools for forgings
FORMING-Coining dies(cold), Cold extrusion dies, punches, Tube and section forming rolls; plain rolls, Cold heading tools, and Master hobs for cold hobbing.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.81 g/cc0.282 lb/in³hardened to 57 HRC
 7.70 g/cc
@Temperature 399 °C
0.278 lb/in³
@Temperature 750 °F
hardened to 57 HRC
 7.75 g/cc
@Temperature 199 °C
0.280 lb/in³
@Temperature 390 °F
hardened to 57 HRC
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 200200Soft annealed (Delivery condition)
Modulus of Elasticity 200 GPa29000 ksi(hardened to 57 HRC)
 179 GPa
@Temperature 399 °C
26000 ksi
@Temperature 750 °F
hardened to 57 HRC
 193 GPa
@Temperature 199 °C
28000 ksi
@Temperature 390 °F
hardened to 57 HRC
Compressive Yield Strength 1380 MPa200000 psi0.2%, hardened to 45 HRC
 1650 MPa239000 psi0.2%, hardened to 50 HRC
 2030 MPa294000 psi0.2%, hardened to 55 HRC
 2070 MPa300000 psi0.2%, hardened to 58 HRC
Charpy Impact 10.8 - 16.3 J8.00 - 12.0 ft-lbAustenitizing temp 1725°F, Tempering temp 400-1000°F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.1 µm/m-°C
@Temperature 199 °C
6.70 µin/in-°F
@Temperature 390 °F
hardened to 57 HRC
 12.4 µm/m-°C
@Temperature 399 °C
6.90 µin/in-°F
@Temperature 750 °F
hardened to 57 HRC
Specific Heat Capacity 0.460 J/g-°C
@Temperature 20.0 °C
0.110 BTU/lb-°F
@Temperature 68.0 °F
hardened to 57 HRC
Thermal Conductivity  28.9 W/m-K
@Temperature 20.0 °C
201 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
hardened to 57 HRC
 30.0 W/m-K
@Temperature 199 °C
208 BTU-in/hr-ft²-°F
@Temperature 390 °F
hardened to 57 HRC
 31.0 W/m-K
@Temperature 399 °C
215 BTU-in/hr-ft²-°F
@Temperature 750 °F
hardened to 57 HRC
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.53 %0.53 %
Chromium, Cr 3.2 %3.2 %
Iron, Fe 93.77 %93.77 %As Balance
Manganese, Mn 0.70 %0.70 %
Molybdenum, Mo 1.5 %1.5 %
Silicon, Si 0.30 %0.30 %
Sulfur, S <= 0.0050 %<= 0.0050 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EDRO #7 Shock Resistant S7 Tool Steel
Carpenter S7 Alloy Tool Steel (AISI S7)
Crucible Steel S7 (AISI S7) Tool Steel
Crucible Steel S7 XL (Premium AISI S7) Tool Steel
Latrobe LSS™ S7 Shock-Resisting Tool Steel (ASTM S7)

NBUCOR13 / 15482

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.