MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Radici Heraflex ® E 6521 1000 NAT Thermoplastic Polyester Elastomer
Categories: Polymer; Thermoplastic; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: TPC-ET Thermoplastic Elastomer. Medium-high modulus, nominal shore D/15s 57. Natural color.

Information provided by Radici Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³ISO 1183
Water Absorption 0.20 %
@Thickness 1.00 mm
0.20 %
@Thickness 0.0394 in
Immersion; ISO 62
Melt Flow 23 g/10 min
@Load 2.16 kg,
Temperature 230 °C
23 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565Instantaneous; ISO 7619-1
 57
@Time 15.0 sec
57
@Time 0.00417 hour
ISO 7619-1
Tensile Strength at Break 38.0 MPa5510 psi5mm / min.; ISO 527-2/1A
Tensile Strength, Yield 25.0 MPa3630 psi50mm/min.; ISO 527-2/1A
 19.0 MPa
@Strain 10 %
2760 psi
@Strain 10 %
ISO 527-2/1A
 22.0 MPa
@Strain 100 %
3190 psi
@Strain 100 %
ISO 527-2/1A
 23.0 MPa
@Strain 300 %
3340 psi
@Strain 300 %
ISO 527-2/1A
Elongation at Break 600 %600 %50 mm / min. Nominal.; ISO 527-2/1A
Elongation at Yield 25 %25 %ISO 527-2/1A
Tensile Modulus 0.390 GPa56.6 ksi1mm / min.; ISO 527-2/1A
Flexural Strength 20.0 MPa2900 psi2mm / min.; ISO 178
Flexural Modulus 0.370 GPa53.7 ksi2mm / min.; ISO 178
Charpy Impact, Notched 7.00 J/cm²33.3 ft-lb/in²ISO 179/1e/A
Tear Strength 241 kN/m1380 pliISO 34-1
Abrasion 2020ISO 4649
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cm500V; IEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohm500V; IEC 60093
 
Thermal PropertiesMetricEnglishComments
Melting Point 212 °C414 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 110 °C230 °FISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FISO 75/2Af
Vicat Softening Point 195 °C
@Load 5.10 kg
383 °F
@Load 11.2 lb
50°C/h; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 230 - 240 °C446 - 464 °FInjection Molding
Mold Temperature 30.0 - 50.0 °C86.0 - 122 °F
 
Descriptive Properties
Injection Molding Injection SpeedMedium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRADI6977 / 293482

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.