MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

GRECO ISOTANE® 3095A-FR TPU Resin, Flame Retardant
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Characteristics: ISOTHANE®FR series products are thermoplastic polyurethane containing halogen-free fire retardant. They not only offer excellent flame retardancy, but also possess good mechanical properties, hydrolytic stability, low temperature flexibility and abrasion resistance. ISOTHANE®FR series can be processed by extrusion and injection molding.

Application: Building/Construction, Mining, Wire and Cables

Information provided by Great Eastern Resins Industrial Co. Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9494ASTM D2240
Tensile Strength 25.0 MPa3630 psiASTM D412
Elongation at Break 400 %400 %ASTM D412
50% Modulus 10.0 MPa10.0 MPaASTM D412
100% Modulus 12.0 MPa1740 psiASTM D412
300% Modulus 19.0 MPa2760 psiASTM D412
Tear Strength 130 kN/m742 pliDie C; ASTM D624
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-0
@Thickness 2.00 mm
V-0
@Thickness 0.0787 in
 
Descriptive Properties
AppearanceWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGRECO5158 / 282141

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.