MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M Scotch® Super 33+™ Vinyl Electrical Tape
Categories: Polymer; Tape; Thermoplastic; Vinyl (PVC)

Material Notes: Scotch® Super 33+™ Vinyl Electrical Tape is a premium grade, 7 mil thick, all-weather vinyl-insulating tape. It is designed to perform continuously in ambient temperatures up to 105°C. The tape is conformable for cold weather application down to -18°C. It has excellent resistance to abrasion, moisture, alkalies, acids, corrosion and varying weather conditions (including ultraviolet exposure). The combination of elastic backing and aggressive adhesive provides moisture-tight electrical and mechanical protection with minimum bulk. Scotch® Super 33+™ Vinyl Electrical Tape is UL Listed and is a Canadian Standards Association (CSA) Certified “Insulating Tape”.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 178 microns7.00 mil
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break  100 %
@Temperature -18.0 °C
100 %
@Temperature -0.400 °F
ASTM D1000
 250 %
@Temperature 22.0 °C
250 %
@Temperature 71.6 °F
ASTM D1000
Peel Strength  0.307 kN/m
@Temperature 2.00 °C
1.75 pli
@Temperature 35.6 °F
Adhesion to Steel; ASTM D1000
 0.307 kN/m
@Temperature 22.0 °C
1.75 pli
@Temperature 71.6 °F
Adhesion to Backing; ASTM D1000
 0.657 kN/m
@Temperature -18.0 °C
3.75 pli
@Temperature -0.400 °F
Adhesion to Steel; ASTM D1000
 0.657 kN/m
@Temperature -18.0 °C
3.75 pli
@Temperature -0.400 °F
Adhesion to Backing; ASTM D1000
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance >= 1.00e+12 ohm>= 1.00e+12 ohmASTM D1000
Dielectric Strength 45.3 kV/mm1150 kV/inASTM D1000
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 105 °C221 °F
Minimum Service Temperature, Air -18.0 °C-0.400 °F
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM35169 / 169916

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.