MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
CoorsTek Hot Pressed Aluminum Nitride
Categories: Ceramic; Nitride

Material Notes: Aluminum Nitride Advantages:
  • High heat dissipation with thermal conductivity of 170 W/m K
  • Non-toxic alternative to BeO
  • Thermal expansion coefficient similar to Si, GaN, and GaAs semiconductors
  • High dielectric strength

Information provided by CoorsTek, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.26 g/ccASTM C20
Water Absorption 0.00 %ASTM 373
Permeability 0.00Gas
 
Mechanical PropertiesOriginal ValueComments
Hardness, Knoop 111000gm
Modulus of Elasticity 330 GPaASTM C848
Flexural Strength 340 MPaMOR, Four point bend modulus of rupture; ASTM F417
Poissons Ratio 0.25ASTM C848
Fracture Toughness 3.00 MPa-m½KIc; Notched Beam
Shear Modulus 132 GPaCalculated
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1000 ohm-cm
@Temperature 1000 °C
ASTM D1829
 >= 1e+05
@Temperature 500 °C
ASTM D1829
 >= 1.00e+13 ohm-cm
@Temperature 25.0 °C
ASTM D1829
Dielectric Constant 9.0
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 17.0 kV/mm
@Thickness 6.35 mm
ASTM D150
Dielectric Loss Index <= 0.0010
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.00 µm/m-°C
@Temperature 25.0 - 1000 °C
ASTM C372
Specific Heat Capacity 0.740 J/g-°C
@Temperature 100 °C
ASTM E1269
Thermal Conductivity 80.0 W/m-KASTM C408
Maximum Service Temperature, Air 800 °CNo load condition

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum Nitride, AlN
CoorsTek AIN-170 Hot Pressed Aluminum Nitride
MarkeTech AN 90 Aluminum Nitride Ceramic Substrate, 98% Purity
CeramTec Alunit® Aluminum Nitride
H.C. Starck Grade A Aluminum Nitride AIN

CCOOR938 / 140553

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.