MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Inhance Fluoro-Seal INHANCE® HD-1800 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: INHANCE HD-1000 Series Polyethylene Particles are surface-activated High Density Polyethylene (HDPE) in particle or powder form. Surface activation makes the particles easy to disperse, and creates superior adhesion between the particles and the surrounding polymer.

Applications: Add INHANCE HD polyethylene to urethanes, epoxies, polyesters, and other polymers to create composites that capture the unique benefits of HDPE. These benefits include excellent abrasion resistance, reduced coefficient of friction, enhanced tear strength and improved moisture barrier. INHANCE HD polyethylene can be used in many applications including molded parts, adhesives, paints, and coatings. It can be used as profile additive that tenaciously bonds to the matrix polymer. INHANCE HD polyethylene is easily dispersed in water-based, solvent, and 100% solids coatings of all types. Typical incorporation levels are in the range of 5% - 40%.

Information provided by Inhance/Fluoro-Seal, Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.930 - 0.940 g/cc
Bulk Density 0.416 - 0.528 g/cc
Particle Size 20 µmAverage Size
 53 µmFiner than
Surface Tension 55 dynes/cmwater wettable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PINHAN007 / 137218

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.