MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Latrobe HS-105™ ASTM M35 DIN 1.3243 High Speed Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Carbon Steel; High Carbon Steel; Tool Steel

Material Notes: HS-105 high speed steel is a cobalt-modified M2 high speed steel in which the cobalt addition provides hot hardness that is intermediate between those of M2 and M42 high speed steels. The improved hot hardness makes the steel suitable for machining high-strength and prehardened steels, high-hardness alloys, and the difficult-to-machine, nonferrous superalloys used in the aerospace, oil, and power generation industries. Typical applications for HS-105 high speed steel include twist drills, taps, milling cutters, reamers, broaches, saws, knives, and hobs.

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 8.14 g/cc8.14 g/cc
Density 8.14 g/cc0.294 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 64.864.8Oil Quenched from 1232°C, 5 minutes
 65.265.2Oil Quenched from 1177°C, 5 minutes
 65.265.2Oil Quenched from 1204°C, 5 minutes
Modulus of Elasticity 207 GPa30000 ksi
Machinability 45 - 50 %45 - 50 %1% Carbon Steel
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.4 µm/m-°C
@Temperature 21.0 - 399 °C
6.33 µin/in-°F
@Temperature 69.8 - 750 °F
 11.5 µm/m-°C
@Temperature 21.0 - 593 °C
6.39 µin/in-°F
@Temperature 69.8 - 1100 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 849 °C1560 °FCritical Temperaure Ac1
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.93 %0.93 %
Chromium, Cr 4.2 %4.2 %
Cobalt, Co 4.9 %4.9 %
Iron, Fe 76.52 %76.52 %
Molybdenum, Mo 5.0 %5.0 %
Silicon, Si 0.30 %0.30 %
Tungsten, W 6.25 %6.25 %
Vanadium, V 1.9 %1.9 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type M35 Molybdenum High Speed Tool Steel (UNS T11335)
Latrobe Double Six™ ASTM M2 High Speed Steel
Crucible Steel CPM® REX® M35HCHS High Speed Steel, AISI M35
AISI Type M2 Molybdenum High Speed Tool Steel (UNS T11302)
Bohler-Uddeholm BÖHLER S601 (M2 Modified) High Speed Steel For Cold Work Applications

NTIMK070 / 19417

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.