3M™ Scotch-Seal™ Industrial Sealant 800 is a reddish brown, brushable sealant that air dries to a flexible seal that resists water, oils and fuel and adheres to many metallic surfaces and has a useful temperature range of -65° to 200°F (-54 to 93°C).Information provided by 3M |