(Viewing data as-entered.
Click here
to return)
3M Scotch-Weld™ 2141 Neoprene Rubber & Gasket Adhesive
Categories:
Polymer
;
Adhesive
Material Notes:
Features:
Alight colored, high strength adhesive with a long tack range
Excellent water, oil and grease resistance
Bonds neoprene, natural, reclaim SB-R and butyl rubber to most substrates.
Information provided by 3M
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Solids Content
28 - 32 %
Brookfield Viscosity
900
-
1500
cP
RVF #2 sp @ 20 rpm @ 80°F
Mechanical Properties
Original Value
Comments
Shear Strength
68.0
psi
@Temperature 82.0 °C,
Time 1.81e+6 sec
Overlap, 1/8" Birch/Birch
377
psi
@Temperature 24.0 °C,
Time 1.81e+6 sec
Overlap, 1/8" Birch/Birch
Peel Strength
6.00
pli
@Temperature 24.0 °C,
Time 86400 sec
180°, Canvas/Steel
10.0
pli
@Temperature 24.0 °C,
Time 259000 sec
180°, Canvas/Steel
14.0
pli
@Temperature -34.0 °C,
Time 1.81e+6 sec
180°, Canvas/Steel
22.0
pli
@Temperature 82.0 °C,
Time 1.81e+6 sec
180°, Canvas/Steel
24.0
pli
@Temperature 66.0 °C,
Time 1.81e+6 sec
180°, Canvas/Steel
24.0
pli
@Temperature 24.0 °C,
Time 432000 sec
180°, Canvas/Steel
30.0
pli
@Temperature 24.0 °C,
Time 1.81e+6 sec
180°, Canvas/Steel
32.0
pli
@Temperature 24.0 °C,
Time 605000 sec
180°, Canvas/Steel
32.0
pli
@Temperature 24.0 °C,
Time 1.21e+6 sec
180°, Canvas/Steel
Thermal Properties
Original Value
Comments
Flash Point
-26.0
°C
TCC
Descriptive Properties
Appearance
Yellow
Base
Polychloroprene
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
3M Scotch-Weld™ 10 Neoprene Contact Adhesive
COR12V Cork/Neoprene Rubber Sheet
Garlock 3206 Neoprene/Polyester Fabric
Polychloroprene Rubber (CR)
Denka Neoprene 671A Polychloroprene
PMM34116 / 168863
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.