MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hyosung Topilene J742S PP
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: J742S Injection Impact Copolymer

Applications: Large articles:

  • Washing M/C parts
  • Electric appliance
  • Industrial appliance
Characteristics:
  • Medium impact
  • High stiffness

Information provided by Hyosung Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 28 g/10 min28 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8585ASTM D785
Tensile Strength, Yield 28.4 MPa4120 psiASTM D638
Elongation at Break 200 %200 %ASTM D638
Flexural Modulus 1.47 GPa213 ksiASTM D790
Izod Impact, Unnotched 0.785 J/cm1.47 ft-lb/inASTM D256
 0.441 J/cm
@Temperature -10.0 °C
0.827 ft-lb/in
@Temperature 14.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C248 °FASTM D648
Vicat Softening Point 150 °C302 °FASTM D1525
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hyosung Topilene HJ640A PP
Hyosung Topilene J800 PP
Hyosung Topilene J301CP PP
Hyosung Topilene HJ746 PP
Hyosung Topilene HJ700 PP

PHYOS08 / 47894

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.