MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Evonik TAGAT® V 20 Emulsifier
Categories: Fluid

Material Notes: TAGAT® V 20 an ethoxylated castor oil oleate, is a non-ionic emulsifier.

Application: The low foaming emulsifier TAGAT® V 20 is used in a wide range of applications such as

  • Metal working fluids (MWF)
  • Concrete release agents
  • Textile auxiliary formulations
  • Pulp and paper defoamers
In the case of metalworking application, TAGAT® V 20 is mainly used for the formulation of environmentally friendly fluids based on vegetable (e. g. rape seed oil) and synthetic ester oils (e. g. trimethylol propane trioleate), as well as combinations of these oils with mineral oils. If TAGAT® V 20 is used with other emulsifiers e. g. alcohol ethoxylates, for the formulation of metalworking fluids, manufacturer recommends a dosage of 3 to 9 %.

Properties / Benefits: TAGAT® V 20 has excellent emulsifying properties and ensures the spontaneous formation of finely dispersed, stable oil-in-water emulsions (o/w). This allows in general a reduction of the total emulsifier content which is necessary for the fluid emulsification. Since TAGAT® V 20 is an emulsifier based on raw materials derived from vegetable oils it exhibits benign properties and hence does not carry a risk phrase:

  • TAGAT® V 20 has good toxicological and ecological properties (water hazard classification = 1)
  • TAGAT® V 20 does not require any hazardous classification in accordance with EG directives/ German regulations on dangerous substances
  • TAGAT® V 20 has good dermatological properties (no skin irritation)

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 7.0[mg KOH/g]
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 1.0 %
 
Descriptive Properties
Appearanceclear liquid
Color<30Hess-Ives
Content7.4-9.4%HLB
Hydroxyl Number43-53 mg KOH/g
Saponification Number100-120 mg KOH/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik SIPERNAT® 383 DS Silica Powder
Evonik BREAK-THRU® AF 9908 Surfactants
Evonik SIPERNAT® D 13 Silica Powder
Evonik SIPERNAT® D 10 Ceramic Powder
Evonik SIPERNAT® 50 Silica Powder

PEVONIL533 / 196737

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.