MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Lubrizol Advanced Materials Stat-Rite® S-608 PETG Alloy
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); PETG Copolyester

Material Notes: Product Description: S-608 is a static dissipative PETG alloy. It utilized the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protection. Stat-Rite® IDP alloys provide consistent static dissipation even when thermoformed or injection molded into components. Features: permanently static dissipative; Humidity Independent; Ultra clean: low out-gassing, low extractable ionics; Durable: can be used for years. Applications: Hard disk drive component packaging; Electronic component packaging; Medical device packaging.
Availability: Asia Pacific, Europe, Latin America, North America
Features: Antistatic; Clean/High Purity; Durable; ESD Protection; Humidity Independent: Low (to None) Ion Content; Low Extractables; Low to No Outgassing; Rapid Static Decay
Uses: Computer Components; Electrical/Electronic Applications; Medical Packaging; Packaging
Appearance: Light Blue
Forms: Sheet
Processing Method: Injection Molding; Thermoforming

Information provided by Lubrizol Advanced Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 28.3 MPa4100 psiASTM D638
Elongation at Break 350 %350 %ASTM D638
Tensile Modulus 1.10 GPa160 ksiASTM D638
Flexural Modulus 1.24 GPa180 ksiASTM D790
Izod Impact, Notched 9.61 J/cm18.0 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.00e+9 ohm-cm5.00e+9 ohm-cmASTM D257
Surface Resistance 5.00e+8 ohm5.00e+8 ohm12% RH; ESD S11.11
Surface Resistivity per Square 2.00e+9 ohm2.00e+9 ohm50% RH; ASTM D257
Static Decay 0.010 sec0.010 sec-5000 V to -50 V, FTMS-101C, 12% RH
 0.010 sec0.010 sec5000 V to 50 V, FTMS-101C, 12% RH
 0.30 sec0.30 sec1000 V to 10 V, CPM, 50% RH
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 60.0 °C140 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C131 °FUnannealed; ASTM D648
 
Descriptive Properties
Ionic Content2.0 ng/cm2F Anion, Test Method #3010-4
 2.0 ng/cm2PO4 Anions, Test Method #3010-4
 3.0 ng/cm2NO3 Anions, Test Method #3010-4
 5.0 ng/cm2SO4 Anions, Test Method #3010-4
 5.0 ng/cm2Cl Anion, Test Method #3010-4
Non-Volatile Content0.5 ng/cm2Test Name #3010-5
Outgassing0.1 µg/gStyrene , Test Method #3010-3
 0.3 µg/gToluene , Test Method #3010-3
 0.8 µg/gMMA , Test Method #3010-3
 4.0 µg/gTotal Organics , Test Method #3010-3
Tribocharge - Nitrile Glove10.0 V

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLUBR6025 / 268327

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.