Chemical description: Polyether emulsion. Application fields: GETREN® L 6000 is a release agent for long hoses extruded on rubber coated or pure plastic mandrels. Additionally GETREN® L 6000 can be used as anti-blocking agent. Advantages: - usable for all common rubber compounds
- silicone-free
- solvent-free
- stable at temperatures up to 200 °C
Information provided by Evonik |