MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trelleborg Emerson & Cuming Eccobond® 56C Two-Component Silver Filled Electrically Conductive Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy, Electrically Conductive

Material Notes: Emerson & Cuming 56C Eccobond® Two-Component Silver Filled Electrically Conductive Epoxy Adhesive
Silver filled, high electrical conductivity, epoxy adhesive. Excellent thermal conductivity. Requires heat cure to obtain optimal properties. Recommended for applications where hot soldering is impractical. Listed on many government specifications. Mix ratio of 100:2.5. Cure Type: Heat Bonding Type: Epoxy

The Eccobond® product line is now a part of Henkel; this specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.50 g/cc
 
Mechanical PropertiesOriginal ValueComments
Adhesive Bond Strength 800 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.00020 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 130 °C
Minimum Service Temperature, Air -40.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 0.500 hour
@Temperature 100 °C
 1.00 hour
@Temperature 65.0 °C
 
Descriptive Properties
ColorSilver
ViscosityThixotropic (Mixed, 25°C)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Abatron 8509-2A/8509-1B Carbon-Filled Electrically Conductive Epoxy Compound
Master Bond EP51AN Thermally Conductive Adhesive System
Trelleborg Emerson & Cuming Eccobond® 23 LV General Purpose Catalyst
Trelleborg Emerson & Cuming Eccobond® 57C Two-Component Silver Filled Electrically Conductive Epoxy Adhesive
Master Bond EP21TDCS Silver Filled Electrically Conductive Epoxy Compound

PEMERS52 / 35744

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.