MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Avient Stat-Tech™ PI-05CF/000 EM Polyetherimide (PEI)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compounds combine the performance of select engineering resins with reinforcing additives such as carbon powder, carbon fiber, nickel-coated carbon fiber and stainless steel fiber, for low-to-high levels of conductivity depending upon application requirements.

Description/Features:

  • PEI (Polyetherimide)
  • 5% Carbon Fiber Reinforced
  • ESD Protection
  • Antistatic
  • Static Dissipative

Applications:

  • EMI?RFI Shielding
  • Printer Components
  • Enclosures
  • Fuel Systems

Processing Method: Injection Molding

Information provided by PolyOne Corporation

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.29 g/ccASTM D792
Water Absorption 0.25 %
@Thickness 3.17 mm
24 hr. Immersion; ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 18000 psiType 1 - Rigids, Yield, 0.2 in/min; ASTM D638
Elongation at Break 4.0 - 5.0 %Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 650000 psiType 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 28000 psiASTM D790
Flexural Modulus 650000 psiASTM D790
Izod Impact, Notched 0.900 ft-lb/in
@Thickness 6.35 mm,
Temperature 23.0 °C
Method A, Injection Molded; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1000 ohm-cm - 1e+05ASTM D257
Surface Resistivity per Square 1000 ohm - 1e+05ASTM D257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 405 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 390 °FUnannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 670 - 720 °FMolding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyetherimide (PEI), 10% Glass Fiber
Overview of materials for Polyetherimide (PEI)
Global PEI-110 Easy Flow, Polyetherimide
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
Overview of materials for Polyetherimide (PEI), 20% Glass Fiber

PH1PO0530a / 43590

Ensinger SPI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.