MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LATI Latene® 7H2W T-V0E PP Homopolymer, Mineral Reinforced, Heat Stabilized, Flame Retardant
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant; Polypropylene, Mineral Reinforced

Material Notes: Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.32 g/cc
Linear Mold Shrinkage, Flow 0.0075 - 0.0095 cm/cm
Linear Mold Shrinkage, Transverse 0.0070 - 0.0090 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 10.0 MPa
@Temperature 90.0 °C
 15.0 MPa
@Temperature 60.0 °C
 25.0 MPa
@Temperature 23.0 °C
Elongation at Break 3.7 %
@Temperature 23.0 °C
 6.0 %
@Temperature 60.0 °C
 10 %
@Temperature 90.0 °C
Elongation at Yield 2.3 %
@Temperature 23.0 °C
 5.5 %
@Temperature 60.0 °C
 6.5 %
@Temperature 90.0 °C
Tensile Modulus 1000 MPa
@Temperature 90.0 °C
 1450 MPa
@Temperature 60.0 °C
 3500 MPa
@Temperature 23.0 °C
Charpy Impact Unnotched 6.50 kJ/m²
@Temperature -20.0 °C
 20.0 kJ/m²
@Temperature 23.0 °C
Charpy Impact, Notched 2.30 kJ/m²
@Temperature -20.0 °C
 2.50 kJ/m²
@Temperature 23.0 °C
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 600 VA solution
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 105 °C
Deflection Temperature at 0.46 MPa (66 psi) 115 °C
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
Vicat Softening Point 70.0 °C
@Load 5.00 kg
Flammability, UL94 V-0
@Thickness 1.50 mm
 V-0
@Thickness 0.750 mm
 5VB
@Thickness 3.00 mm
Oxygen Index 27 %
Glow Wire Test 960 °C
@Thickness 1.00 mm
GWFI/GWT
 960 °C
@Thickness 2.00 mm
GWFI/GWT
 
Processing PropertiesOriginal ValueComments
Melt Temperature 180 - 220 °C
Mold Temperature 20.0 - 40.0 °C
Drying Temperature 80.0 - 90.0 °C
@Time 10800 sec
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polykemi AB POLYfill PPH T8020 Polypropylene Homopolymer, Mineral Reinforced
LATI Latene® 7H2W-V0 PP Homopolymer, Heat Stabilized, Flame Retardant
Celanese SO.F.TER Forprene® 6NM.A45 TPE
LATI Latene® AG3H2W G/30-V0E PP Homopolymer, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant

PLATH9763 / 177459

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.