ALPLAN® 5083 precision plates exhibit good dimensional stability. Their low internal stresses reduces the effects of plate deformation during machining, thus saving on extra operations such as rough-milling, furnishing or re-work. Surface milling by the end user is not necessary. Applications include reference plates, control tools, jigs.Information provided by manufacturer |
EN AW-5083; Al Mg4.5Mn0.7 |