MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Niche Polymer POLIXL™ PPHGF40BK PPH, 40% Fiberglass Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Glass Fiber Filler

Material Notes:

Information provided by Niche Polymer

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0020 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.0030 cm/cmASTM D955
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
Ash 40 %glass-fiber; ASTM D2584
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 96.0 MPaISO 527
Elongation at Break 3.0 %ISO 527
Flexural Strength 148 MPaISO 178
Flexural Modulus 6750 MPaISO 178
Izod Impact, Notched (ISO) 11.5 kJ/m²ISO 180
 
Thermal PropertiesOriginal ValueComments
Melting Point 162 °C
Deflection Temperature at 0.46 MPa (66 psi) 157 °CUnannealed; ISO 75
Flammability, UL94 HB
@Thickness 1.50 mm
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Owens Corning Glass Fiber Reinforced Polyester BMC (Injection), 22 wt.% glass
Owens Corning Glass Fiber Reinforced Polyester (Spray-up/Lay-up), 30 wt.% glass
Owens Corning Glass Fiber Reinforced Polyester (Pultruded), 55 wt.% glass
Niche Polymer POLIXL™ PPCGF40BK PPC, 40% Fiberglass Reinforced
Mocom (ALBIS) Altech® NXT PP PP-H A 2040/456.01 LE GF40 CP 40% Glass Filled PP Homopolymer

PNICHE172 / 193754

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.