MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lion SBR 4503C Elastomer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Hot polymerized SBR 4503C is used in construction mastics, adhesives and sealants intended for installing panels, furring strips, wood molding, plywood or hardboard. It offers a strong and instant bond that retains precise placement. It exhibits excellent shear strength and yields a stiffer film when used in tape, PSA or label application.

Unique Features:

  • Hot polymerized SBR terpolymer
  • Moderate crosslinking reduces shrinkage
  • Higher bound Styrene content
Applications:
  • Construction adhesives and mastics
  • Pressure-sensitive label and tape adhesives
  • Mechanical rubber goods and bead wire adhesives

Information provided by Lion Elastomer

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.990 g/ccASTM D-792
Volatiles <= 0.75 %ZS 1008K
Viscosity 110 - 400 cP4% Toluene solution
Ash <= 1.5 %
 
Chemical PropertiesOriginal ValueComments
Styrene Content 28.5 - 31.5 %Bound
 
Thermal PropertiesOriginal ValueComments
Shrinkage <= 35 %Mill
 
Descriptive Properties
ColorOff White
Content<0.5%Soap
 4-6%Organic acid
 5-11%Total dust, Calcium Carbonate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLION080 / 317989

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.