MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
TIMET TIMETAL® 685 (Ti-6Al-5Zr-0.5Mo-0.25Si) Titanium Alloy
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Near Alpha Titanium Alloy

Material Notes: High-Temperature, High-Strength Creep Resistant Alloy

Industry Specifications: Germany Aerospace: 3.7154. France: T-A6ZD. UK Aerospace Specifications BS TA. 43, 44.

Features: TIMETAL 685 possesses excellent tensile strength and creep resistance up to 520°C. It is weldable and has good forging characteristics. The alloy may be joined by the processes normally used in the fabrication of titanium, including argon-arc, electron beam and friction welding. Material should be fully heat treated prior to welding, and also given a suitable post-weld treatment. The weld zone of material treated in this way will have similar structure and properties to the parent metal. This alloy was specifically designed for the aero-engine industry. It is nonmagnetic.

Typical heat treatment for this alloy: Solution heat treatment: 1050°C for 30 mins, oil quench. Aging heat treatment: 550°C for 24 hours, air cool.

Data provided by TIMET.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 4.45 g/ccTypical
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 1030 MPaTypical
Tensile Strength, Yield 900 MPa
@Strain 0.2 %
Typical
Elongation at Break 10 %Typical in 5D
Reduction of Area 20 %
Modulus of Elasticity 125 GPaTypical
Notched Tensile Strength 1648 MPaKt=3
Poissons Ratio 0.33Calculated by MatWeb
Fatigue Strength 440 MPa
@# of Cycles 1.00e+7
alternating direct-stress (zero mean stress)
 630 MPa
@# of Cycles 100000
alternating direct-stress (zero mean stress)
Fracture Toughness 68.0 MPa-m½K(IC); Typical
Shear Modulus 47.0 GPa
Charpy Impact 43.0 J
@Diameter 25.0 mm
rod
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000167 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.50 µm/m-°C
@Temperature 20.0 - 300 °C
 9.70 µm/m-°C
@Temperature 20.0 - 100 °C
 10.1 µm/m-°C
@Temperature 20.0 - 500 °C
Thermal Conductivity 4.15 W/m-K
Maximum Service Temperature, Air 520 °CGood creep resistance
Beta Transus 1020 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 5.7 - 6.3 %
Carbon, C <= 0.080 %
Iron, Fe <= 0.050 %
Molybdenum, Mo 0.25 - 0.75 %
Nitrogen, N <= 0.030 %
Oxygen, O <= 0.20 %
Silicon, Si 0.015 - 0.35 %
Titanium, Ti 85.8 - 89.5 %Calculated as remainder
Zirconium, Zr 4.5 - 6.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Annealed Sheet/Plate & Billet/Bar
Titanium IMI 685 (Ti-6Al-5Zr-0.5Mo-0.25Si)
Titanium Ti-6Al-4V (Grade 5), Annealed
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Beta Forged
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Beta Rolled plus Mill Annealed

NTIME685 / 19337

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.