MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Polyester Film
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyester Film". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 - 1.51 g/ccAverage value: 1.37 g/cc Grade Count:390
Brightness 85.0 - 115 %Average value: 102 % Grade Count:12
Water Absorption 0.150 - 0.800 %Average value: 0.384 % Grade Count:9
Moisture Vapor Transmission 0.0120 - 1.20 cc-mm/m²-24hr-atmAverage value: 0.583 cc-mm/m²-24hr-atm Grade Count:126
Water Vapor Transmission 4.00 - 104 g/m²/dayAverage value: 29.1 g/m²/day Grade Count:31
 0.776 - 43.456 g/m²/day
@Temperature 38.0 - 38.0 °C
Average value: 23.9 g/m²/day Grade Count:33
Oxygen Transmission 0.0200 - 44.0 cc-mm/m²-24hr-atmAverage value: 2.87 cc-mm/m²-24hr-atm Grade Count:130
Carbon Dioxide Transmission 149 - 211 cc-mm/m²-24hr-atmAverage value: 170 cc-mm/m²-24hr-atm Grade Count:3
Viscosity 800000 - 800000 cP
@Temperature 270 - 270 °C
Average value: 800000 cP Grade Count:1
 800000 - 800000 cP
@Shear Rate 100 - 100 1/s
Average value: 800000 cP Grade Count:1
Thickness 2.54 - 478 micronsAverage value: 73.3 microns Grade Count:493
Surface Tension 8.00 - 47.0 dynes/cmAverage value: 33.1 dynes/cm Grade Count:3
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 81.0 - 95.0Average value: 86.3 Grade Count:9
Tensile Strength, Ultimate 23.0 - 200 MPaAverage value: 53.1 MPa Grade Count:8
Film Tensile Strength at Yield, MD 35.2 - 228 MPaAverage value: 92.8 MPa Grade Count:139
Film Tensile Strength at Yield, TD 27.6 - 228 MPaAverage value: 92.8 MPa Grade Count:135
Film Elongation at Break, MD 74.0 - 440 %Average value: 135 % Grade Count:472
Film Elongation at Break, TD 55.0 - 445 %Average value: 101 % Grade Count:454
Film Elongation at Yield, MD 5.00 - 12.0 %Average value: 7.80 % Grade Count:5
Film Elongation at Yield, TD 5.00 - 20.0 %Average value: 9.40 % Grade Count:5
Elongation at Break 130 - 830 %Average value: 678 % Grade Count:8
Modulus of Elasticity 3.10 - 4.36 GPaAverage value: 3.65 GPa Grade Count:72
Flexural Yield Strength 138 MPaAverage value: 138 MPa Grade Count:3
Flex Crack Resistance 15000 - 20000Average value: 18100 Grade Count:8
Poissons Ratio 0.380 - 0.580Average value: 0.480 Grade Count:13
Secant Modulus 3.79 GPaAverage value: 3.79 GPa Grade Count:91
Secant Modulus, MD 1.46 - 6.35 GPaAverage value: 2.60 GPa Grade Count:16
Secant Modulus, TD 1.38 - 7.02 GPaAverage value: 2.69 GPa Grade Count:15
Puncture Energy 1.60 - 4.60 JAverage value: 3.83 J Grade Count:4
 0.700 - 1.20 J
@Temperature -20.0 - 0.000 °C
Average value: 0.950 J Grade Count:1
Coefficient of Friction 0.200 - 1.48Average value: 0.401 Grade Count:164
Coefficient of Friction, Static 0.280 - 0.600Average value: 0.411 Grade Count:78
Tear Strength Test 0.700 - 600Average value: 73.2 Grade Count:112
Tear Strength 9.00 - 140 kN/mAverage value: 47.7 kN/m Grade Count:10
Graves Tear Strength 0.123 - 233 kN/mAverage value: 20.7 kN/m Grade Count:21
Elmendorf Tear Strength MD 377 - 724 gAverage value: 533 g Grade Count:4
Elmendorf Tear Strength TD 428 - 897 gAverage value: 627 g Grade Count:4
Elmendorf Tear Strength, MD 0.827 - 7.09 g/micronAverage value: 2.95 g/micron Grade Count:6
Elmendorf Tear Strength, TD 0.866 - 5.30 g/micronAverage value: 2.49 g/micron Grade Count:5
Dart Drop 3.20 - 3.53 g/micronAverage value: 3.41 g/micron Grade Count:3
 3.20 - 3.65 g/micron
@Temperature -30.0 - -18.0 °C
Average value: 3.42 g/micron Grade Count:3
Dart Drop Test 825 - 882 gAverage value: 863 g Grade Count:3
 825 - 913 g
@Temperature -30.0 - -18.0 °C
Average value: 874 g Grade Count:3
Seal Strength 102 - 3000 g/25 mmAverage value: 583 g/25 mm Grade Count:10
Film Tensile Strength at Break, MD 41.0 - 284 MPaAverage value: 177 MPa Grade Count:516
Film Tensile Strength at Break, TD 35.0 - 314 MPaAverage value: 216 MPa Grade Count:495
Heat Seal Strength 22.0 - 1800 g/25 mmAverage value: 441 g/25 mm Grade Count:14
Heat Seal Strength Initiation Temperature 104 - 204 °CAverage value: 159 °C Grade Count:7
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+8 - 1.00e+18 ohm-cmAverage value: 1.03e+17 ohm-cm Grade Count:32
Surface Resistance 10.0 - 2.00e+17 ohmAverage value: 6.74e+15 ohm Grade Count:41
Dielectric Constant 2.43 - 3.20Average value: 2.87 Grade Count:18
Dielectric Strength 14.6 - 410 kV/mmAverage value: 157 kV/mm Grade Count:81
 200 - 200 kV/mm
@Temperature 150 - 150 °C
Average value: 200 kV/mm Grade Count:1
 200 - 200 kV/mm
@Frequency 50.0 - 50.0 Hz
Average value: 200 kV/mm Grade Count:1
Dielectric Breakdown 490 - 26000 VAverage value: 10800 V Grade Count:74
Dissipation Factor 0.00300 - 0.0550Average value: 0.0121 Grade Count:11
Arc Resistance 131 - 135 secAverage value: 133 sec Grade Count:4
Comparative Tracking Index 400 - 600 VAverage value: 500 V Grade Count:28
Hot Wire Ignition, HWI 7.00 - 15.0 secAverage value: 8.71 sec Grade Count:28
High Amp Arc Ignition, HAI 15.0 - 120 arcsAverage value: 60.0 arcs Grade Count:28
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.0 - 90.0 µm/m-°CAverage value: 31.5 µm/m-°C Grade Count:26
 17.0 - 17.0 µm/m-°C
@Temperature 30.0 - 50.0 °C
Average value: 17.0 µm/m-°C Grade Count:13
Specific Heat Capacity 1.17 J/g-°CAverage value: 1.17 J/g-°C Grade Count:172
 1.29704 - 2.59408 J/g-°C
@Temperature 60.0 - 250 °C
Average value: 1.95 J/g-°C Grade Count:7
Thermal Conductivity 0.150 - 0.155 W/m-KAverage value: 0.154 W/m-K Grade Count:14
Melting Point 220 - 269 °CAverage value: 254 °C Grade Count:193
Crystallization Temperature 170 - 175 °CAverage value: 173 °C Grade Count:3
Maximum Service Temperature, Air 65.0 - 232 °CAverage value: 146 °C Grade Count:197
Deflection Temperature at 0.46 MPa (66 psi) 68.0 - 71.0 °CAverage value: 69.5 °C Grade Count:4
Deflection Temperature at 1.8 MPa (264 psi) 62.0 - 64.0 °CAverage value: 62.8 °C Grade Count:4
Vicat Softening Point 79.0 - 81.0 °CAverage value: 80.5 °C Grade Count:4
Minimum Service Temperature, Air -73.3 - -40.0 °CAverage value: -49.9 °C Grade Count:134
Brittleness Temperature -60.0 - -40.0 °CAverage value: -48.3 °C Grade Count:3
Glass Transition Temp, Tg 35.0 - 150 °CAverage value: 87.5 °C Grade Count:15
UL RTI, Electrical 160 °CAverage value: 160 °C Grade Count:3
UL RTI, Mechanical without Impact 180 °CAverage value: 180 °C Grade Count:3
Flammability, UL94 HBGrade Count:3
Oxygen Index 23.5 - 24.7 %Average value: 24.1 % Grade Count:4
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.54 - 1.67Average value: 1.65 Grade Count:123
Optical Density 0.500 - 46.0Average value: 15.8 Grade Count:20
Haze 0.180 - 97.0 %Average value: 12.8 % Grade Count:294
Gloss 1.30 - 200 %Average value: 78.0 % Grade Count:99
Yellow Index -1.50 - 0.500 %Average value: -0.167 % Grade Count:3
Transmission, Visible 1.10 - 96.0 %Average value: 76.3 % Grade Count:225
UV Transmittance 8.00 - 89.0 %Average value: 57.2 % Grade Count:5
 
Processing PropertiesOriginal ValueComments
Processing Temperature 93.0 - 220 °CAverage value: 185 °C Grade Count:19
Melt Temperature 223 - 282 °CAverage value: 244 °C Grade Count:5
Cure Time 90.0 - 90.0 min
@Temperature 177 - 177 °C
Average value: 90.0 min Grade Count:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyester (Thermoset) - Rigid
Overview of materials for Polyester Thermoplastic Elastomer
Overview of materials for Low Density Polyethylene (LDPE), Film Grade
Overview of materials for Nylon 66, Film
Saint-Gobain Norton® PVDF Fluoropolymer Film

O3475 / 78216

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.