Product Description: Grilamid L 20 HL black 9563 is a, medium viscosity extrusion grade, based on Polyamide 12 (PA12). Grilamid L20 HL black 9563 has been especially developed for external cable sheathing applications, it is UV-stabilized, heat stabilized as it is resistant to termites. The special features of Grilamid L 20 HL black 9563 are:- Maximum UV-resistance
- Heat stability
- Resistant to termites
- Good chemical resistance
- Good resistance to il
- High surface quality
- High abrasion resistance
- Good dimensional stability
- Easy to process
- Low density, low weight
Application examples: Grilamid L 20 HL black 9563 is suitable for the outer sheathing layer of telecommunication cables.Information provided by EMS Grivory. |