MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ho Hsiang Ching HN-6065W SEBS
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: The HN series belongs to the SEBS (STYRENE-ETHYLENE/BUTYLENE- STYRENE) hydrogenated and alloyed grade of materials. The HN series, it specialized in PA(Nylon) over-molding, has excellent weather resistance, heat temperatures resistance on processing and extraordinary anti-scratch. The HN series texture is dry and comfortable; in addition to forming, the HN series always performs well in a double layer injection when bonds with PA6 and PA66 material. For example, when using pneumatic or power tools, nylon is required as the main material due to its different characteristics and structure, however, in order to enhance a soft grip comfort and a sense of design, the material must not only be soft, but also have good binding properties. Our HN series has overcome the problem of high temperatures injection and bonded- molded, its virtues develop the good performance in the field of pneumatic tools, power tools and sporting products. Suitable for most of the thermoplastic processing methods, such as injection molding, extrusion molding and so on. This material complies with EU RoHS specifications , REACH-SVHC and has passed the Nylon Phenol Ethoxylates (NPEO), Polynuclear Aromatic Hydrocarbons (PAHs) and other safety tests.

Color: Natural Color / Black Color / Customized Color

The optimum combination of materials: PA (Nylon)

Processing: Injection, Extrusion

Storage conditions: At room temperature, avoid direct sunlight, keep away from fire and avoid humid environment.

Applications: Sport goods, pneumatic tools, power tools, etc

Information provided by Ho Hsiang Ching Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.880 g/cc0.880 g/ccASTM D792
Melt Flow 83 g/10 min
@Load 5.00 kg,
Temperature 200 °C
83 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070ASTM D2240
Tensile Strength 3.24 MPa469 psiASTM 412C
Elongation at Break 465 %465 %ASTM 412C
Tear Strength 31.4 kN/m179 pliASTM 412C
 
Thermal PropertiesMetricEnglishComments
Heat Distortion Temperature 100 °C212 °F
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 160 - 177 °C320 - 351 °F
Middle Barrel Temperature 166 - 182 °C331 - 360 °F
Front Barrel Temperature 177 - 191 °C351 - 376 °F
Nozzle Temperature 182 - 204 °C360 - 399 °F
Mold Temperature 16.0 - 66.0 °C60.8 - 151 °F
Injection Velocity 13.0 - 25.0 mm/sec0.512 - 0.984 in/sec
Injection Pressure 34.0 - 69.0 MPa4930 - 10000 psi
Hold Pressure 14.0 - 48.0 MPa2030 - 6960 psi
Back Pressure 0.340 - 0.690 MPa49.3 - 100 psi
Screw Speed 50 - 70 rpm50 - 70 rpm
 
Descriptive Properties
Cold resistance temperature-50°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHSIANG044 / 312520

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.