MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Jilin Xingyun Chemical XY-1 Yield increase agent for delayed coking and coke inhibition
Categories: Other Engineering Material

Material Notes: This product mixed with raw material in fluid coker, after chemical reaction and physical change, it could not only enhance the coking liquid yield, but also restrain the coking in furnace tube by extending production cycle and coking cycle and enhancing economic efficiency. This product is an oil-soluble liquid, which is not corrosive to equipment, easy added, no effect to the load of equipment..

Information provided by Jilin Xingyun Chemical Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.850 - 0.950 g/cc0.0307 - 0.0343 lb/in³
Kinematic Viscosity 40 - 200 cSt40 - 200 cStDynamic
 
Thermal PropertiesMetricEnglishComments
Solidus <= -20.0 °C<= -4.00 °F
Flash Point >= 50.0 °C>= 122 °F
 
Descriptive Properties
AppearanceBrown Liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PJILINX060 / 317907

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.