System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
SABIC LNP™ STAT-LOY™ Compound M3000 Polypropylene, Unspecified (PP, Unspecified) (Americas)
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
Material Notes:
LNP STAT-LOY M3000 compound is based on unfilled Polypropylene (PP) resin containing proprietary fillers. Added features of this grade include: Permanently Anti-Static.
Features: Antistatic
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.950
g/cc
0.0343
lb/in³
ASTM D792
0.950
g/cc
0.0343
lb/in³
ISO 1183
Moisture Absorption
0.850 %
0.850 %
23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow
0.0135
cm/cm
0.0135
in/in
24hrs; ISO 294
0.014
cm/cm
0.014
in/in
24hrs; ASTM D955
Linear Mold Shrinkage, Transverse
0.013
cm/cm
0.013
in/in
24hrs; ASTM D955
0.0133
cm/cm
0.0133
in/in
24hrs; ISO 294
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
28.0
MPa
4060
psi
ASTM D638
28.0
MPa
4060
psi
ISO 527
Elongation at Break
47 %
47 %
ASTM D638
98.2 %
98.2 %
ISO 527
Elongation at Yield
8.0 %
8.0 %
ISO 527
9.6 %
9.6 %
ASTM D638
Tensile Modulus
1.35
GPa
196
ksi
1 mm/min; ISO 527
1.39
GPa
202
ksi
50 mm/min; ASTM D638
Flexural Strength
32.0
MPa
4640
psi
ISO 178
40.0
MPa
5800
psi
ASTM D790
Flexural Modulus
1.36
GPa
197
ksi
ISO 178
1.44
GPa
209
ksi
ASTM D790
Izod Impact Notched
69.0
J
50.9
ft-lb
ASTM D256
Izod Impact, Unnotched
NB
NB
ASTM D4812
Izod Impact, Notched (ISO)
10.0
kJ/m²
4.76
ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO)
NB
NB
80*10*4; ISO 180/1U
Dart Drop, Total Energy
7.00
J
5.16
ft-lb
peak; ASTM D3763
Impact Test
5.00
J
3.69
ft-lb
Multiaxial Impact; ISO 6603
Electrical Properties
Metric
English
Comments
Surface Resistance
1.00e+9
-
1.00e+11
ohm
1.00e+9
-
1.00e+11
ohm
ASTM D257
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
110
µm/m-°C
@Temperature -40.0 - 40.0 °C
61.1
µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
110
µm/m-°C
@Temperature -40.0 - 40.0 °C
61.1
µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow
128
µm/m-°C
@Temperature -40.0 - 40.0 °C
71.1
µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
128
µm/m-°C
@Temperature -40.0 - 40.0 °C
71.1
µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi)
103
°C
217
°F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
100
°C
@Thickness 3.20 mm
212
°F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
59.0
°C
138
°F
Flatw 80*10*4 sp=64mm; ISO 75/Af
56.0
°C
@Thickness 3.20 mm
133
°F
@Thickness 0.126 in
unannealed; ASTM D648
Processing Properties
Metric
English
Comments
Zone 2
195
-
205
°C
383
-
401
°F
Zone 3
200
-
210
°C
392
-
410
°F
Melt Temperature
190
-
200
°C
374
-
392
°F
Injection Molding
Mold Temperature
30.0
-
50.0
°C
86.0
-
122
°F
Drying Temperature
70.0
-
80.0
°C
158
-
176
°F
Injection Molding
Dry Time
4.00
hour
4.00
hour
Injection Molding
Back Pressure
0.200
-
0.300
MPa
29.0
-
43.5
psi
Screw Speed
30
-
60
rpm
30
-
60
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PSABH81416 / 289363
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.