MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol Advanced Materials PEARLTHANE® 12K92A Thermoplastic Polyurethane Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: PEARLTHANE® 12K92A is a standard polyester-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties. It can be extruded. PEARLTHANE® 12K92A is used for the extrusion of films in general and especially adhesive films, either flat or blown films.

All information provided by Merquinsa

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.22 g/cc1.22 g/ccASTM D792
Melt Flow 10 g/10 min
@Load 21.6 kg
10 g/10 min
@Load 47.6 lb
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9494ASTM D2240
Tensile Strength 35.06 MPa5085 psiASTM D412
Elongation at Break 500 %500 %ASTM D412
100% Modulus 11.00 MPa
@Strain 100 %
1595 psi
@Strain 100 %
ASTM D412
300% Modulus 22.03 MPa
@Strain 300 %
3195 psi
@Strain 300 %
ASTM D412
Tear Strength 120 kN/m685 pliASTM D624 (Die C)
Abrasion 2525loss (mm³); DIN 53.516
 
Thermal PropertiesMetricEnglishComments
Melting Point 165 - 175 °C329 - 347 °FMQSA 111
Glass Transition Temp, Tg -13.9 °C7.00 °FDSC, 10ºC/min; DIN 51.007
 
Processing PropertiesMetricEnglishComments
Zone 1 150 - 180 °C302 - 356 °F
Zone 2 160 - 190 °C320 - 374 °F
Zone 3 170 - 200 °C338 - 392 °F
Zone 4 175 - 205 °C347 - 401 °F
Die Temperature 175 - 200 °C347 - 392 °F
Moisture Content <= 0.10 %<= 0.10 %MQSA 44

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled
Lubrizol ISOPLAST™ 202EZ Engineering Thermoplastic Polyurethane Resin
Lubrizol Advanced Materials PEARLTHANE® 12K85A Thermoplastic Polyurethane Elastomer
Celanese Celstran® TPU-GF60-01-US TPU, 60% Glass Reinforced

PMES56 / 88433

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.