MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lehvoss LUVOCOM® 19-7744 VP Polyamide 46 with aramid reinforcement and PTFE
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 46 (PA46)

Material Notes: Properties/attributes include: Good friction and wear behavior especially at high temperatures. Emergency-running capability.

Automotive industry, textile- and office machinery, apparatus- and precision engineering. Typical uses include: Bearings, sleeves, sliding elements, control disks, gear wheels, duty parts in switches.

Processing: During processing the moisture level should not exceed 0.1%, otherwise molecular degradation and surface defects (e.g. smearing) may occur. Excessively high predrying temperatures may cause discoloration. The processing notes provided merely represent a recommendation for general use. Due to the large variety of machines, geometries and volumes of parts, etc., it may be necessary to employ different settings according to the specific application.

Information provided by Lehmann & Voss & Co.KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/ccISO 1183
Moisture Absorption <= 1.00 %
@Temperature 23.0 °C,
Time 86400 sec
<= 1.00 %
@Temperature 73.4 °F,
Time 24.0 hour
Linear Mold Shrinkage 0.013 - 0.020 cm/cm0.013 - 0.020 in/inDIN 16901
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 65.0 MPa9430 psiISO 527-2
Elongation at Break 5.0 %5.0 %ISO 527-2
Modulus of Elasticity 2.90 GPa421 ksiISO 527-2
Flexural Strength 95.0 MPa13800 psiISO 178
Flexural Modulus 2.60 GPa377 ksiISO 178
Flexural Strain at Break 6.5 %6.5 %Flexural Elongation @ Fmax; ISO 178
Charpy Impact Unnotched 3.20 J/cm²
@Temperature 23.0 °C
15.2 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eU
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+12 ohm-cm>= 1.00e+12 ohm-cmIEC 60167
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C302 °FContinuous; UL 746B
 160 °C320 °FShort Term
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 280 - 330 °C536 - 626 °F
Zone 1 285 - 315 °C545 - 599 °F
Zone 2 305 - 315 °C581 - 599 °F
Zone 3 305 - 315 °C581 - 599 °F
Melt Temperature 310 °C590 °F
Mold Temperature 90.0 - 130 °C194 - 266 °F
Drying Temperature  80.0 °C
@Time 7200 - 28800 sec
176 °F
@Time 2.00 - 8.00 hour
Dehumidifying dryer
 80.0 °C
@Time 7200 - 43200 sec
176 °F
@Time 2.00 - 12.0 hour
Vacuum Dryer
Moisture Content <= 0.10 %<= 0.10 %
 
Descriptive Properties
Colornatural color (beige)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLUU8903 / 193862

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.