Availability: Asia Pacific; Europe; North America Additive: Heat Stabilizer; Impact Modifier Features: Good Toughness; Heat Stabilized; Impact Modified; Medium Viscosity Automotive Specifications: FORD ESB-M4D178-A2; GM GMP.PA6.005 Color: Black; GM GMP.PA6.005 Color: Natural Form: Pellets Processing Method: Injection Molding Information provided by Teknor Apex |