Product Description: LLB2019 has exceptional toughness and strength and ease of extrusion. Applications for LLB2019 include trash bags, liners, general packaging, industrial liners, heavy duty bags, stretch wrap, blend resin and industrial packaging. Availability: North America Additive: Antiblock: No; Processing Aid; Yes; Slip: No Features: Good Toughness; High Strength Uses: Bags; Heavy-duty Bags; Industrial Applications; Liners; Packaging; Stretch Wrap Processing Method: Extrusion Information provided by Osterman & Company |