MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

SABIC LNP™ COLORCOMP™ Compound WX96084-WH9A496 Polybutylene Terephthalate (PBT)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: LNP COLORCOMP WX96084-WH9A496 compound is based on Polybutylene Terephthalate (PBT) resin. Added features of this grade include: Custom Color White WH9A496.

Features: Aesthetics and Appearance,Custom Color

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.50 g/cc1.50 g/ccASTM D792
Density 1.50 g/cc0.0542 lb/in³ISO 1183
Water Absorption 0.080 %
@Time 86400 sec
0.080 %
@Time 24.0 hour
ASTM D570
Moisture Absorption 0.0100 %0.0100 %23°C/50% RH/24 hrs; ASTM D570
 0.0300 %0.0300 %23°C / 50% RH; ISO 62
 0.0500 %0.0500 %Injection Molding
Water Absorption at Saturation 0.13 %0.13 %ISO 62-1
Viscosity 87 cP
@Load 5.00 kg,
Temperature 265 °C
87 cP
@Load 11.0 lb,
Temperature 509 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.023 cm/cm0.023 in/inSABIC method
Linear Mold Shrinkage, Transverse 0.022 cm/cm0.022 in/inSABIC method
Melt Flow 130 g/10 min
@Load 5.00 kg,
Temperature 265 °C
130 g/10 min
@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 40.0 MPa5800 psi5 mm/min; ASTM D638
 40.0 MPa5800 psi5 mm/min; ISO 527
Tensile Strength, Yield 41.0 MPa5950 psi5 mm/min; ASTM D638
 45.0 MPa6530 psi5 mm/min; ISO 527
Elongation at Break 22 %22 %5 mm/min; ASTM D638
 22 %22 %5 mm/min; ISO 527
Elongation at Yield 22 %22 %5 mm/min; ISO 527
 30 %30 %5 mm/min; ASTM D638
Tensile Modulus 2.05 GPa297 ksi5 mm/min; ASTM D638
 2.10 GPa305 ksi1 mm/min; ISO 527
Flexural Strength 61.0 MPa8850 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
 65.0 MPa9430 psiyield, 2 mm/min; ISO 178
Flexural Modulus 1.80 GPa261 ksi1.3 mm/min, 50 mm span; ASTM D790
 1.90 GPa276 ksi2 mm/min; ISO 178
Izod Impact Notched 100 J73.8 ft-lbASTM D256
Izod Impact, Unnotched NBNBASTM D4812
Izod Impact, Notched (ISO) 13.5 kJ/m²6.42 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NBNB80*10*4; ISO 180/1U
Charpy Impact Unnotched NBNBEdgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 3.00 J/cm²14.3 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 150 µm/m-°C
@Temperature 23.0 - 60.0 °C
83.3 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 150 µm/m-°C
@Temperature 23.0 - 60.0 °C
83.3 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 125 °C257 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 53.0 °C127 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 50.0 °C
@Thickness 3.20 mm
122 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 180 °C356 °FRate B/50; ASTM D1525
 180 °C356 °FRate B/50; ISO 306
 
Processing PropertiesMetricEnglishComments
Zone 2 245 - 255 °C473 - 491 °F
Zone 3 260 - 270 °C500 - 518 °F
Melt Temperature 240 - 265 °C464 - 509 °FInjection Molding
Mold Temperature 80.0 - 100 °C176 - 212 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80584 / 288531

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.