MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Tra-Con Tra-Bond F118CLR Fiber Optic Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND F118CLR is an impact resistant, fiber-optic adhesive designed for use in any optical connector. This two-part epoxy remains at a constant viscosity for a minimum of 30 minutes. This allows more connectors to be produced from one mix. Low stress, TRA-BOND F118CLR is an excellent choice for multi and single mode connectors where excessive curing temperatures may cause cracking. It can be cured at room temperature overnight or as fast as 15 minutes at 65°C. The clear color facilitates easy polishing and its cured properties prevent pistoning. This 100% solid system can be used for small potting and sealing applications where resistance to thermal shock and impact are required. This system can be supplied in many different packages including 2 gram (or larger) BlPAX kits, pre-mixed and frozen syringes or 1 gram MINIPAX. Variations on viscosity (or other properties) are available upon request. Longer cures may be required for development of full mechanical properties in potting or sealing applications. Sufficient cure is developed for polishing connectors in 15 minutes at 65°C. TRA-BOND F118CLR will complete its cure at room temperature with no pistoning.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/ccMixed
Viscosity 65000 cP
@Temperature 25.0 °C
65000 cP
@Temperature 77.0 °F
After mixing
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8282
Adhesive Bond Strength 23.4 MPa3400 psiLap shear, alum to alum
Izod Impact, Notched 0.117 J/cm0.220 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 130 °C266 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
Glass Transition Temp, Tg 105 °C221 °FUltimate Tg
 
Processing PropertiesMetricEnglishComments
Cure Time  15.0 min
@Temperature 90.0 °C
0.250 hour
@Temperature 194 °F
1 drop applications
 60.0 min
@Temperature 65.0 °C
1.00 hour
@Temperature 149 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Pot Life 30 min30 min
 
Descriptive Properties
Color Hazy, Off White
Mix Ratio, parts by weight100/30Resin/Hardener
Working Life hours 1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTRAC231 / 71159

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.