MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Crosspolimeri GETILAN 04/AF3 Thermoplastic, halogen free, flame retardant compound
Categories: Polymer; Thermoplastic

Material Notes: GETILAN: flexible thermoplastic compound halogen free and flame retardant.

GETILAN 04/AF3: thermoplastic, low smoke, halogen free, flame retardant compound for cables sheathing and insulation It is studied to produce a general purpose flexible sheathing without migration risks (plasticizers-free).

Certify: TI6, TM7, VDE 0207 HM4(K=0,7), AS/NZS 3808:2000 HFI 75-90 TP, HFS 75-90-110 TP, IEC 60092-359 SHF1

Information provided by Crosspolimeri S.P.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.51 g/ccASTM D792
Melt Flow 1.0 - 6.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
Storage Temperature 12.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 41ASTM D2240
Tensile Strength >= 9.00 MPaIEC 60811
 >= 6.00 MPa
@Temperature 110 °C,
Time 648000 sec
Heat Ageing; AS-3808-200
Elongation at Break >= 200 %IEC 60811
 >= 100 %
@Temperature 110 °C,
Time 648000 sec
Heat Ageing; AS-3808-200
 
Thermal PropertiesOriginal ValueComments
Hot Ball Pressure Test 90.0 °C
@Time 21600 sec
<50%, Residual Value, (K=0.7); IEC 60811
Oxygen Index >= 31 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Zone 1 145 °C
Zone 2 160 °C
Zone 3 185 °C
Zone 4 190 °C
Die Temperature 205 °C
Head Temperature 200 °C
Dry Time 3.00 hour
@Temperature 80.0 °C
 4.00 hour
@Temperature 80.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCROS126 / 294210

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.