MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
TIMCAL TIMREX® GB98/75 Natural Graphite
Categories: Carbon; Graphite; Other Engineering Material; Additive/Filler for Polymer

Material Notes: TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-des-Îles, Quebec, Canada. Further processing can be done either in Lac-des-Îles or for high added value products (e.g. TIMREX PG25) in our new processing plant in Terrebonne, Quebec, Canada. All TIMREX

“Naturals” are thoroughly controlled in our laboratories to ensure quality, consistency and total customer satisfaction.

Tribological and mechanical properties:

  • Very good lubrication properties
Advantages and applications:
  • Very low friction coefficient
  • Low wear of the counterpart
  • Very high electrical conductivity
  • Suitable for semimetallic and metallic brushes
Information provided by TIMCAL

Key Words: CAS Number 7782-42-5
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Size 5.0 µmat a density of 1.91 g/cc
 5.0 µmSpringback 9.5%, pressure 0.477 t/cc
 10 µmat a density of 2.00 g/cc
 40 µmat a density of 2.10 g/cc
 60 µmat a density of 2.11 g/cc
 60 µmSpringback 5%, pressure 0.477 t/cc
Ash 1.3 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00 ohm-cmparticle size 60 um, pressure 2.5 t/cc
 1.45 ohm-cmparticle size 18 um, pressure 2.5 t/cc
 1.85 ohm-cmparticle size 5 um, pressure 2.5 t/cc
 
Component Elements PropertiesOriginal ValueComments
H2O, Water 0.10 %
 
Descriptive Properties
Crystallinity Height Lc>400 nm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
TIMCAL TIMREX® C-LUB 302 Primary Synthetic Graphite
TIMCAL TIMREX® KS6 Primary Synthetic Graphite
TIMCAL TIMREX® LSG6 Natural Graphite
TIMCAL TIMREX® M150 mesh Natural Flake Graphite
TIMCAL TIMREX® FC250 Coke

CTIMCAL51a / 140849

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.