MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Silastic® 9201-50 LSR Oil-Bleeding Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Standard grade, oil-filled, self-lubricating LSR. SILASTIC™ 920x-yy Series LSRs where x = oil content and yy = Durometer hardness.

Product applications:

  • Automotive connector seals
  • Electrical connections
  • Weatherpack seals
Key Features:
  • Oil filled
  • Low compression set
  • Low viscosity
  • Unique rheology
  • Opaque

Former Dow Corning brand.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.12 g/cc1.12 g/ccASTM D792
Viscosity  140000 cP
@Frequency 10 Hz
140000 cP
@Frequency 10 Hz
Part B; CTM 1094
 180000 cP
@Frequency 10 Hz
180000 cP
@Frequency 10 Hz
Part A; CTM 1094
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050ASTM D2240
Tensile Strength 7.20 MPa1040 psiASTM D412
Elongation at Break 400 %400 %ASTM D412
Tear Strength 40.0 kN/m228 pliASTM D624 DIE B
Compression Set 21 %
@Temperature 175 °C,
Time 79200 sec
21 %
@Temperature 347 °F,
Time 22.0 hour
NPC; ASTM D395
 
Descriptive Properties
Oil Content. Weight %1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOW9930 / 233133

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.