System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Arkema Nakan® RRS 401 L PVC, Rigid Injection Grade
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Vinyl (PVC)
;
PVC, Rigid Grade
Material Notes:
NAKAN RRS 401 L is a rigid polyvinyl chloride compound developed for injection molding of waste water fittings.
ISO data provided by the manufacturer, Arkema.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.41
g/cc
Mechanical Properties
Original Value
Comments
Tensile Strength, Yield
55.0
MPa
50 mm/min
Elongation at Break
25 %
Nominal Strain; 50 mm/min
Elongation at Yield
5.0 %
50 mm/min
Tensile Modulus
2.70
GPa
1 mm/min
Charpy Impact Unnotched
NB
Charpy Impact, Notched
0.400
J/cm²
Thermal Properties
Original Value
Comments
Deflection Temperature at 1.8 MPa (264 psi)
64.0
°C
Vicat Softening Point
73.0
°C
50°C/hr; 50N
Flammability, UL94
V-0
@Thickness 1.60 mm
Oxygen Index
46 %
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Arkema Nakan® RMA 705 N PVC, Rigid Injection Molding Grade
Arkema Nakan® RMS 501 L PVC, Rigid Injection Molding Grade
Colorite Polymers 2007F Rigid PVC
Karina 802-18/462-C-ERB Gray PVC Compound
Teknor Apex Sinvicomp SRF 3703 Polyvinyl Chloride, Rigid
PZARKG400 / 25694
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.