MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
China-Yixing Longly Refractories 95 Alumina Ceramic
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: LONGLY selects high quality ceramic fine powder and micropowder as materials, adopts modern advanced molding technology to produce a multitude of ceramic tubes, rods, beads, balls, columns, plates, films and other forms. These ceramic products sintered in high temperature has a large elastic modulus, high mechanical strength, high oxidation resistance at elevated temperatures, excellent thermal conductivity, good electrical insulation, high electric strength, low dielectric loss, stability of electric properties with temperature and frequency variation, high wear-resistance, good corrosion resistance, superior waterproof under temperature mutation and surface machinability. Many of alumina's extinguished properties could be strengthened through variation in manufacturing methods and in chemistry.

Applications: Widely used in electronics, electrical appliances, machinery, petroleum, chemical, medical, textile, automobile, metallurgy and aerospace industries and so on.

Information Provided by China Yixing Longly Refractories Co. Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.50 - 3.60 g/cc
Water Absorption <= 0.080 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 9.0
Flexural Strength >= 520 MPacold bending
Compressive Strength >= 500 MPaAmbient
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cm
@Temperature 100 °C
Dielectric Strength 15.0 kV/mmInsulating Strength
 17.6 - 20.0 kV/mmDC Breakdown Strength
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.50 - 7.80 µm/m-°C
@Temperature 25.0 - 800 °C
Thermal Conductivity 26.0 W/m-K
Maximum Service Temperature, Air >= 1500 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 92 - 96 %
 
Descriptive Properties
Refractoriness (°C)>2000

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
China-Yixing Longly Refractories 99 Alumina Ceramic
COI Ceramics Nextel™ A-N720 Oxide Ceramic Matrix Composite, Alumina
China-Yixing Longly Refractories 75 Alumina Ceramic
Chosun Refractories SFC-90W High-Alumina Castable
Chosun Refractories SFC-90SC High-Alumina Castable

CYXLR016 / 99318

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.