MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Lubrizol Estane® L194A Thermoplastic Polyurethane  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Type: Estane® L194A is a Shore 95A, polyester grade thermoplastic polyurethane (TPU).

Uses: Injection Molding.

Availability: Asia

Information Provided by The Lubrizol Corporation

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Linear Mold Shrinkage 0.0080 cm/cm0.0080 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9494ASTM D2240
Hardness, Shore D 5252ASTM D2240
Tensile Strength, Ultimate 41.2 MPa5970 psiASTM D412
Tensile Strength, Yield 13.7 MPa1990 psi100% elongation; ASTM D412
 29.4 MPa4270 psi300% elongation; ASTM D412
Elongation at Break 440 %440 %ASTM D412
100% Modulus 13.7 MPa
@Strain 100 %
1990 psi
@Strain 100 %
ASTM D412
300% Modulus 29.4 MPa
@Strain 300 %
4260 psi
@Strain 300 %
ASTM D412
Tear Strength 167 kN/m952 pliDie C; ASTM D624
Compression Set  15 %
@Temperature 23.0 °C,
Time 79200 sec
15 %
@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
 40 %
@Temperature 70.0 °C,
Time 79200 sec
40 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 130 °C266 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Feed Temperature 185 - 200 °C365 - 392 °F
Nozzle Temperature 200 - 215 °C392 - 419 °F
Mold Temperature 10.0 - 40.0 °C50.0 - 104 °F
Drying Temperature 70.0 - 80.0 °C158 - 176 °F
Dry Time 4.00 - 5.00 hour4.00 - 5.00 hour
Injection Pressure 11.7 - 15.9 MPa1700 - 2300 psi
Hold Pressure 8.27 - 12.4 MPa1200 - 1800 psi
Back Pressure 0.207 - 0.552 MPa30.0 - 80.0 psi
Cycle Time - Injection 25 - 35 sec25 - 35 sec
Screw Speed 180 - 200 rpm180 - 200 rpm
 
Descriptive Properties
Injection Time (s)12-18
Metering Zone195-210°C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Estane® CS195A Thermoplastic Polyurethane
BASF Elastollan® S 50 A SPF TPUR
Lubrizol Estane® AG 9550 Thermoplastic Polyurethane
Lubrizol Estane® CS190A Thermoplastic Polyurethane
Lubrizol Estane® R185A Thermoplastic Polyurethane

PNOVEON508 / 121399

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.