MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker ELASTOSIL® LR 3271/45 A/B Liquid Silicone Rubber with Low Frictional Coefficient
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Self-adhesive liquid silicone rubbers of the ELASTOSIL® LR 3271 series are paste-like, easily-pigmentable two-component compounds with extremely short curing times.

Properties: ELASTOSIL® LR 3271 series are primerless, selfbonding grades that adhere to various plastic substrates (e.g. PET, PBT) and metals, but not in the mold. The bonding is improved by a subsequent heat treatment process (e.g. four hours at 100 °C). Because of the individual surface properties each substrate must be tested before mass production. If necessary one has to check the development of adhesive properties over time and/or in an environment relevant to the application. The vulcanizates are noted for good mechanical and electrical properties.

Application: ELASTOSIL® LR 3271 series are particularly suitable for the economical production of large series of overmolded parts (thermoplastic/elastomer), even in a comolding process (shuttle mold) under standard conditions, without any special treatment of the mold surface. ELASTOSIL® LR 3271 series has been particularly designed for sanitary applications and shows excellent bonding performance to Polyesters and significantly improved hot water hydrolysis resistance of the adhesion layer. Parts made from ELASTOSIL® LR 3271 can generally be used for technical applications without postcuring. Postcured parts can be used for food contact applications and are suitable for use under the Recommendation "XV. Silicones" of the BfR and FDA § 177.2600 under observance of any given limitations on extractable and volatile substances.

Information provided by Wacker.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/ccISO 1183-1 A
Viscosity 1.30e+6 cP
@Shear Rate 1.00 1/s
DIN 53019
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 45DIN 53505
Tensile Strength 8.00 MPaDIN 53504 S 1
Elongation at Break 590 %DIN 53504 S 1
Rebound 54 %DIN 53512
Tear Strength 114 pliASTM D 624 B
Compression Set 10 %
@Temperature 125 °C,
Time 79200 sec
after 4h/100°C post curing; DIN ISO 815-B
 45 %
@Temperature 125 °C,
Time 79200 sec
DIN ISO 815-B
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %Transparent, but not quantified
 
Descriptive Properties
AppearanceTransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Silastic® 25784-V SILICONE RUBBER RED
Aearo E-A-R Specialty Composites VersaDamp™ V-2325 TPE
Overview of materials for Polyester Thermoplastic Elastomer
Elkem (Bluestar Silicones) BLUESIL™ CATA 3038 Silicone Rubber
A. Schulman DuraGrip™ DGR 6030 NC/BK Thermoplastic Elastomer (TPE)

PWACK9930 / 197529

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.