MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Röchling Durostone® UPR S19 Vinyl Ester Components
Categories: Polymer; Thermoset; Vinyl Ester

Material Notes: Durostone® EPR S19 is a threaded rod made of VE-resin and glass fiber using the Sheet-Molding-Compound-Technology (SMC).
  • VE-resin for high dielectric requirements
  • Partial discharge free up to high electric field strength
  • High tracking resistance CTI 600
  • Sizes up to 52 and 4200 mm are possible

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.95 g/ccISO 1183 meth 1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 400 MPaParallel; ASTM D5083
Modulus of Elasticity 20.0 GPaPerpendicular; ISO 178
Flexural Strength 350 MPaPerpendicular; ISO 178
Compressive Strength 450 MPaPerpendicular; ASTM D695
Charpy Impact, Notched 200 kJ/m²Parallel; ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+10 ohmIEC 60093
Dielectric Constant 5.0
@Frequency 48.0 - 62.0 Hz
IEC 60250
Dielectric Strength 15.0 kV/mm
@Temperature 90.0 °C
Parallel; IEC 60243-1
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.0 - 20.0 µm/m-°C
Thermal Conductivity 0.300 W/m-KISO 8302
Maximum Service Temperature, Air 155 °CThermal Endurance; IEC 60216
 
Descriptive Properties
Delamination load4000 NDIN 53463
Insulating classFIEC 60085

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PROCH9107 / 232810

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.