MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay CYCOM® 977-3 Neat Epoxy Resin
Categories: Polymer; Thermoset; Epoxy

Material Notes: CYCOM® 977-3 is a 350°F (177°C) curing resin. It is a toughened epoxy resin with 350°F (177°C) dry and 270°F (132°C) wet service capability. CYCOM 977-3 is formulated for autoclave or press molding and can be cured at 350°F (177°C) for six hours. Unidirectional tape and woven fabric impregnated with CYCOM 977-3 resin will retain tack for 21 days at 72°F (22°C). It has a long mechanical out life suitable for fabrication of large structures.

Features & Benefits:

  • 350°F (177°C) cure
  • Available on fabric and tape
  • 350°F (177°C) dry service temperature
  • 270°F (132°C) wet service temperature
  • Laminate and sandwich panel usage
  • Autoclave or press mold processing
  • Toughened epoxy using proprietary “cocontinuous”morphology
  • Impact resistance
  • Shelf life of 12 months at 0°F (-18°C), 21 days at 72°F (22°C)
Applications:
  • Aircraft primary and secondary structure
  • Applications where impact resistance is critical
  • Applications where hot/wet performance is crucial
Note 1: 5 Harness Satin (5HS) Standard Modulus Carbon Fiber [33 msi (228 GPa)]
Note 2: Typical Unidirectional Tape Properties Intermediate Modulus Carbon Fiber [40 msi (276 GPa)]

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.29 g/cc
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 9600 - 10400 psi
@Temperature 121 °C
wet
 17000 - 25000 psi
@Temperature 24.0 °C
Flexural Modulus 0.300 - 4.50 GPa
@Temperature 121 °C
wet
 3.73 - 3.87 GPa
@Temperature 24.0 °C
Compressive Yield Strength 26.7 - 27.3 ksi
@Temperature 24.0 °C
Fracture Toughness 0.820 - 0.980 MPa-m½K1C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 132 °Cwet
 177 °Cdry
Glass Transition Temp, Tg 178 °CG' DMA at 5°C/min.
 189 °CG" DMA at 5°C/min.
 190 °CTan Delta DMA at 5°C/min.
 
Processing PropertiesOriginal ValueComments
Processing Temperature 350 °FCure
Shelf Life 0.630 Month
@Temperature 22.2 °C
 12.0 Month
@Temperature -17.8 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay CYCOM® 977-20 Resin System with PRIFORM™ Technology
Solvay CYCOM® 7714A Epoxy - Unidirectional Carbon Tape and Roving Composite
Henkel Hysol Benzoxazine 99110 Infusion Resin
Solvay CYCOM® 977-2 Neat Epoxy Resin
Solvay CYCOM® 5276-1 Epoxy with G40-800 Tape Composite

PCYTED091 / 180393

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.