MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco Quenchtex® B
Categories: Fluid; Lubricant

Material Notes: Texaco Quenchtex oils deliver value through:
  • Controlled cooling of metals — Combines the high initial quenching speed of water with slow final quenching speed of oil.
  • Safety — High flash point and fire point minimize the possibility of fire problems.
  • Stable additive package — Minimal loss of additives due to extended use.
  • Minimal oil carryout — The light viscosity of this oil allows quick drainage from metal parts preventing carryout.
  • Excellent thermal stability — Provides high heat resistance to oxidation and thickening.
  • Deeper, more uniform hardening due to controlled cooling of metals.

Texaco Quenchtex oils are highly refined, paraffinic based quenching oils.

They provide controlled cooling of steel which is important in steel hardening. When quenching is started, Texaco Quenchtex oils provides a high initial cooling rate inducing maximum hardness, yet once the critical transformation temperature is passed, the ideal fluid cooling rate decreases to eliminate the possibility of stresses and metal distortion.

Texaco Quenchtex B is recommended where rapid cooling as well as oxidation control is needed.

These oils resist the oxidizing effects of quenching and are less sensitive to the effects of agitation. They are highly heat resistant. No additive replacement is required and, in normal service, they retain the original viscosity indefinitely.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 220565; MSDS Number: 10316

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 33.8 °
Viscosity Measurement 100Viscosity Index
Saybolt Viscosity at 100°F 126 SUS
Saybolt Viscosity at 210°F 42 SUS
Kinematic Viscosity at 40°C (104°F) 23.9 cSt
Kinematic Viscosity at 100°C (212°F) 4.0 cSt
 
Thermal PropertiesOriginal ValueComments
Pour Point -12.0 °C
Flash Point 208 °C
 220 °C[°C] Fire Point
 
Descriptive Properties
Quench Time, s16

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ChevronTexaco Quenchtex® A

WTEXA289 / 77168

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.