MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Fibre Glast 549 Kevlar® Fabric
Categories: Other Engineering Material; Composite Fibers; Polymer; Thermoset; Aramid

Material Notes: This was one of the first high strength synthetic fibers to gain acceptance in the reinforced plastic industry. Unlike the previous synthetic reinforcing fibers, Kevlar® has a considerably higher tensil strength and modulus than fiberglass. Kevlar® is usually used for structures requiring good stiffness, high abrasion resistance, and light weight. Current applications include lightweight boat hulls such as kayaks and canoes, aircraft fuselage panels and pressure vessels. Kevlar® may be used with epoxy or vinyl ester resins.

General Properties for Kevlar®/Carbon Hybrid: Excellent thermal & dimensional stability; Performs with no strength loss up to temperatures of 320°F for extended periods; Lighter in weight than E-Glass with higher specific strengths; Sensitive to direct exposure from UV light; however, demonstrates little or no change in a composite when it is indirectly exposed to UV light; Will not melt or support combustion, however, it will begin to caramelize at approximately 800°F

General Properties for Kevlar®/Carbon Hybrid: Excellent thermal & dimensional stability; Performs with no strength loss up to temperatures of 320°F for extended periods; Lighter in weight than E-Glass with higher specific strengths; Sensitive to direct exposure from UV light; however, demonstrates little or no change in a composite when it is indirectly exposed to UV light; Will not melt or support combustion, however, it will begin to caramelize at approximately 800°F

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 12.0 mil
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 320 °FExtended periods
 
Descriptive Properties
Weave Pattern4-Harness Satin
Weight (oz/sq yd)5
Yarn Description, Fill1140 Denier Kevlar® 49
Yarn Description, Warp1140 Denier Kevlar® 49

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont™ Kevlar® 49 Aramid Fiber
Titanium 11 (Ti-6Al-2Sn-1.5Zr-1Mo-0.35Bi-0.1Si), Aged
DuPont™ Kevlar® 149 Aramid Fiber, diam. 12 µm
DuPont™ Kevlar® 29 Aramid Fiber
Fibre Glast 2443 Kevlar® Twill Weave Fabric

PFIBRE106 / 104543

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.