MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SAE J431 heavy duty automotive gray cast iron, SAE grade G2500a
Categories: Metal; Ferrous Metal; Cast Iron; Gray Cast Iron

Material Notes: If Carbon or Silicon is on the high % range end, the other should be on the low % end. Alloying elements not listed may be required. Properties determined from as-cast test bar 30.5 mm diameter. Microstructure: size 2 to 4 type A graphite in a matrix of lamellar pearlite containing not more than 15% free ferrite. Applications include brake drums and clutch plates for moderate service requirements, where high carbon iron is desired to minimize heat checking. 910 kg minimum transverse load, 4.3 mm minimum deflection.

Key Words: UNS F10009, ferritic, pearlitic, soft iron castings
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.15 g/ccTypical for Gray Cast Iron
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 170 - 229
Hardness, Knoop 222Converted from Brinell
Hardness, Rockwell C 11.4Approximated. Converted from Brinell hardness. Value below normal HRC range, for comparison purposes only.
Hardness, Vickers 209Approximated. Converted from Brinell hardness.
Tensile Strength, Ultimate >= 173 MPa
 
Component Elements PropertiesOriginal ValueComments
Carbon, C >= 3.4 %
Iron, Fe 94 %
Manganese, Mn 0.60 - 0.90 %
Phosphorus, P 0.12 %
Silicon, Si 1.6 - 2.1 %
Sulfur, S 0.12 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SAE J431 automotive gray cast iron, SAE grade G1800
SAE J431 automotive gray cast iron, SAE grade G2500
Gray Cast Iron, ASTM A 48 Class 40
SAE J431 automotive gray cast iron, SAE grade G4000
SAE J431 automotive gray cast iron, SAE grade G3000

MCFE06 / 10400

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.