MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman Eastar GN119 PETG Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); PETG Copolyester

Material Notes: Applications:
  • Personal care and Cosmetics

Product Description: Eastar GN119 Copolyester is a low-I.V. PETG, for sale only in Asia as a high-flow formulation. This product has been GREENGUARD INDOOR AIR QUALITY CERTIFIED®.

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.27 g/ccASTM D792
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 107ASTM D785
Tensile Strength at Break 24.0 MPaASTM D638
Tensile Strength, Yield 48.0 MPaASTM D638
Elongation at Break 75 %ASTM D638
Elongation at Yield 4.0 %ASTM D638
Flexural Strength 66.0 MPaASTM D790
Flexural Modulus 1900 MPaASTM D790
Izod Impact, Notched 46.0 J/m
@Temperature -40.0 °C
ASTM D256
 84.0 J/m
@Temperature 23.0 °C
ASTM D256
Izod Impact, Unnotched NB
@Temperature 23.0 °C
ASTM D4812
 NB
@Temperature -40.0 °C
ASTM D4812
Puncture Energy 35.0 J
@Temperature 23.0 °C
At Max load; ASTM D3763
 44.0 J
@Temperature -40.0 °C
At Max load; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 68.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °CASTM D648
 
Optical PropertiesOriginal ValueComments
Haze 0.40 %ASTM D1003
Transmission, Visible 91 %Total; ASTM D1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 249 - 271 °C
Mold Temperature 16.0 - 38.0 °C
Drying Temperature 71.0 °C
Dry Time 6 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eastman Eastar GN071 Natural PETG Copolyester
Eastman Tritan™ EX401 Copolyester
Eastman Eastar GN007 PETG Copolyester
Eastman Tritan™ MX711 Medical Grade Copolyester
Eastman Tritan™ MX731 Medical Grade Copolyester

PE8810 / 129655

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.