MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Copper-Zinc-Bismuth, Copper Alloy, UNS C49255, H01 Temper, Bar
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: 1/4 Hard

Good Suitability – Soldering, Brazing; Fair Suitability – Capacity for Being Cold Worked; Fair Suitability – Capacity for Being Hot Formed

Typical Uses: Electric and electronic parts; Forgings

Applicable Specifications: Forgings, Die (Hot Pressed) – ASME SB283, ASTM B283/B283M; Rod, Bar & Shapes – Forgings ASTM B124/B124M; Rod, Bar & Wire – ASTM B967/B967M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.304 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 120
@Load 0.500 kg
Tensile Strength 62.0 ksiTypical
 59.0 - 69.0 ksi
Tensile Strength, Yield 42.0 ksi0.2% Offset, Typical
 36.0 - 49.0 ksi0.2% Offset
Elongation at Break 30 %
Tensile Modulus 13700 ksi
Modulus of Rigidity 5000 ksi
Compressive Strength 186.7 ksi0.1 in. set/in.
Poissons Ratio 0.36
Fatigue Strength 34800 psi
@# of Cycles 1.00e+8
Machinability 91 %
Forgeability 90 %
Shear Strength 30.5 ksi
Impact Test 3.30 ft-lb
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000710 ohm-cm24.3% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 34.7 µin/in-°F
@Temperature 20.0 - 100 °C
 36.9 µin/in-°F
@Temperature 20.0 - 200 °C
 39.2 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0910 BTU/lb-°F
Thermal Conductivity 54.7 BTU-in/hr-ft²-°F
Melting Point 880 - 1643 °F
Solidus 880 °F
Liquidus 1643 °F
Annealing Point >= 788 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 428 °FStress Relief
 
Component Elements PropertiesOriginal ValueComments
Bismuth, Bi 1.7 - 2.9 %
Cadmium, Cd <= 0.0075 %
Copper, Cu 58 - 60 %
Iron, Fe <= 0.10 %
Lead, Pb <= 0.090 %
Nickel, Ni <= 0.30 %
Phosphorus, P <= 0.10 %
Selenium, Se 0.020 - 0.070 %
Silicon, Si <= 0.10 %
Tin, Sn <= 0.50 %
Zinc, Zn 35.9 - 40.3 %As Balance

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC49255x1 / 292062

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.