MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ STAT-KON™ Compound EX01407C Polyetherimide (PEI)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: LNP STAT-KON EX01407C compound is based on Polyetherimide (PEI) resin containing carbon fiber and PTFE. Added features of this grade include: LNP Clean Compounding Technology, Electrically Conductive.

Features: LNP Clean Compound Technology,Light-weight Structural,High Heat Resistance,Super Strong (Carbon Fiber Filled),Wear resistant,Electrically Conductive

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/ccASTM D792
Density 1.399 g/cc0.05054 lb/in³ASTM D792
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.130 %0.130 %23°C/50% RH/24 hrs; ASTM D570
 0.200 %0.200 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0055 cm/cm0.0055 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0077 cm/cm0.0077 in/in24hrs; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 88.0 MPa12800 psi5 mm/min; ASTM D638
 89.0 MPa12900 psi5 mm/min; ISO 527
Elongation at Break 2.0 %2.0 %5 mm/min; ASTM D638
 2.0 %2.0 %5 mm/min; ISO 527
Tensile Modulus 10.32 GPa1497 ksi1 mm/min; ISO 527
 11.22 GPa1627 ksi5 mm/min; ASTM D638
Flexural Strength 140 MPa20300 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
 147 MPa21300 psiISO 178
Flexural Modulus 8.95 GPa1300 ksi1.3 mm/min, 50 mm span; ASTM D790
 9.64 GPa1400 ksi2 mm/min; ISO 178
Izod Impact Notched 58.0 J42.8 ft-lbASTM D256
Izod Impact, Unnotched 2.73 J/cm5.11 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 16.0 kJ/m²7.61 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 15.0 J11.1 ft-lbASTM D3763
Impact Test 3.00 J2.21 ft-lbMultiaxial Impact; ISO 6603
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 100 - 1.00e+6 ohm100 - 1.00e+6 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 14.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
7.78 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow 38.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
21.1 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 216 °C421 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 214 °C
@Thickness 3.20 mm
417 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 209 °C408 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 209 °C
@Thickness 3.20 mm
408 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 365 - 375 °C689 - 707 °F
Zone 2 360 - 370 °C680 - 698 °F
Zone 3 365 - 375 °C689 - 707 °F
Melt Temperature 360 - 375 °C680 - 707 °FInjection Molding
Mold Temperature 140 - 180 °C284 - 356 °F
Drying Temperature 150 °C302 °FInjection Molding
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Vent Depth 0.00250 - 0.00760 cm0.000984 - 0.00299 in
 
Descriptive Properties
Screw speed (Circumferential speed)0.2-0.3 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81281 / 289228

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.