MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chengdu Letain LTP ZE-2601 PPS, Al2O3/GF 30% reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: Precise molding materials –LTPZE- 2600 serials LTPZE- 2600 serials reinforced by nano-Al2O3 made a breakthrough on 0.2mm ultra-thin molding. The molding product is smooth and brightness with the surface flexing low than 1% , and can meet the dimension precision requirement of parts and shells for high level electric appliances,

Information provided by Chengdu Letain Plastic

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.65 g/cc0.0596 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 180 MPa26100 psi
Elongation at Break 1.2 %1.2 %
Izod Impact, Notched (ISO) 12.0 kJ/m²5.71 ft-lb/in²
 
Descriptive Properties
flexing deformation1.0 mm
Flow length8 mm
Melt index120-150 g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHENGLT025 / 255878

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.