MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics TR® 19 HS Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Crystalline Silica. TR-19HS Block are asbestos-free insulation products, manufactured from vermiculite granules and high-temperature bonding materials. TR-19HS Block is a high strength structural insulation material, suitable particularly where mechanical loads are present. This block product has very low shrinkage to its 1900°F (1040°C) operating temperature limit and is resistant to cryolite vapor conditions. TR Block products can be manufactured in special shapes to fit customer specifications, saving money on both installation and energy costs. Curved Block Insulation is designed primarily for interior and exterior use on bustle pipes, hot air pipes, stacks and other curved or circular equipment.

Applications:

  • Side and end wall insulating material in carbon baking pits
  • Backup insulation in aluminum pot cells, reheat and pusher furnaces, copper reverberatory furnaces, and oil-fired water tube boilers
  • Interior and exterior use on bustle pipes, hot air pipes, stacks and other curved or circular equipment.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.529 g/ccASTM C 303
 0.561 g/cc
@Temperature 1038 °C
dried; ASTM C 303
Porosity 85 %ASTM C493
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.00120 GPadried; ASTM C 203
Compressive Strength 1.70 MPaCold Crushing Strength, dried; ASTM C 165
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.200 BTU/lb-°F
Maximum Service Temperature, Air <= 1038 °CContinuous Use
 
Descriptive Properties
Colorbeige
Permanent Reheat Shrinkage1.5[%], ASTM C356, fired 24 hours at 1038°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Ceramic Fiber High Temperature Boards M Ceramic Fiber
Unifrax Fiberfrax® LTC HSA™ Systems Ceramic Fiber Insulation
Nurel Engineering Polymers Promyde® B30 P2 GFC15 PA 6, Conditioned, 15% Glass Reinforced, Injection Molded and Heat Stabilized
Morgan Advanced Ceramics Superwool® Pumpable Pumpable
Morgan Advanced Ceramics Ceramic Fiber High Temperature Boards L Ceramic Fiber

CMORF6102 / 202886

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.