MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay MTM® 28 series Epoxy Matrix Resin
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: MTM28 series prepregs are based on 120°C(248°F) curing toughened, epoxy matrix resins that have been specifically developed for the manufacture of components requiring high damage tolerance.

Features & Benefits:

  • Versatile processing: autoclave, oven vacuum bag and press molding
  • 30 days out life at 21°C (70°F)
  • 12 months storage at -18°C(0°F)
  • 85 to 160°C (185 to 320°F) cure
  • Good tack and drape
  • Excellent impact resistance
  • Excellent adhesion to core materials
  • 80°C (176°F) end use temperature
Product Variants:
MTM28B: Black pigmented version of MTM28
MTM28-1: Formatted for unidirectional fiber reinforcement
MTMT28-1B: Black pigmented version of MTM28-1
MTM28-2: Lower tack level
MTM28-2B: Black pigmented version of MTM28-2
MTM28-3: Higher grab characteristic for tube rolling
MTM28-3B: Black pigmented version of MTM28-3
MTM28-3: Higher viscosity
MTM28-4B: Black pigmented version of MTM28-4
MTM28-5: Very low tack level
MTM28-5B: Black pigmented version of MTM28-5

Note 1: Material: MTM28-1/t700-36% RW; Cure cycle: 1 hour at 120°C (248°F), 6.2 bar (90 psi)

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.21 g/ccCured resin, 1 hr at 120°C
Storage Temperature -18.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 8040 psi90°, Note 1; ASTM D3039
 397000 psi0°, Note 1; ASTM D3039
Tensile Modulus 8.40 GPa90° Tensile, Note 1; ASTM D3039
 127 GPa0° Tensile, Note 1; ASTM D3039
Flexural Strength 258000 psi0°, Note 1; CRAG 200
Flexural Modulus 117 GPa0°, Note 1; CRAG 200
Compressive Strength 1309 MPa0°, Note 1; ASTM D695 (MOD)
Compressive Modulus 116000 MPa0°, Note 1; ASTM D695 (MOD)
Shear Modulus 3.69 GPa±45 Interlaminar, Note 1; ASTM D3518
Shear Strength 12600 psi0° Interlaminar, Note 1; ASTM D2344
 18400 psi±45 In-plane, Note 1; ASTM D3518
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 100 °CDMA E' onset Tg, 1 hr at 120°C
 
Processing PropertiesOriginal ValueComments
Cure Time 7.00 min
@Temperature 160 °C
 15.0 min
@Temperature 150 °C
 25.0 min
@Temperature 140 °C
Shelf Life 12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay MTM® 71 Epoxy Matrix Resin
Solvay MTM® 79 Epoxy Matrix with 50% CF1420 Carbon Fiber Composite
Hexcel® HexPly® 8552 Epoxy Matrix
Hexcel® HexPly® 8551-7 Epoxy Matrix
Hexcel® HexPly® M32 Epoxy Matrix

PCYTED145 / 180447

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.