MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lendell Medisponge®
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Latex Free

This line of foam is specifically directed towards the medical industry. This line has regulatory approval under FDA Guidelines 10993-1.

Applications:

Surgeons Blankets, Swabs, Wraps, Wipes, Electronic Cleanroom Wipes, Saliva Swab Kits, Industrial Scrubbers, Foam with "Super Absorbents", Enzymes in Foam, Humidor Sponges, Wicking Sponges, Foot Products, Wound Dressing, Contraceptives, Hydration Products, Medicated Foot Products, Effluent Water Filtrations, Nuclear Waste Filtration

Information provided by Lendell Manufacturing Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 5.70 lb/ft³
Water Absorption 17.2 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 24.6 psiASTM D3574
Elongation at Yield 354.7 %
Tear Strength 5.10 pliDie "C", average; ASTM D3574
 14.1 pliAverage; ASTM D3574
 <= 14.4 pliMax.; ASTM D3574
Compression Set 2.3 %50%; 1H%ct
 4.4 %50%; 1H%cd
 42.9 %50%; 2E%ct
 43.9 %50%; 1A%ct
 80.2 %50%; 1A%cd
 84.5 %50%; 2E%cd
 
Descriptive Properties
% Volume Swell56Saturated
CLD 50%0.7
CLD 50% R0.7
Comfort Factor0.35
Expansion, %13in Isopropyl Alcohol
Hysteresis14.3
IFD 25% R22ASTM D3574
IFD 25% RRT18.9ASTM D3574
IFD 65%63.6ASTM D3574
Recovery85.7
Sag Factor2.9
Water Retention, %2.9
Wet Out, minutes1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lendell Supersoft Foams
Mearthane Durethane™ C Foams DCF and DCM Polyurethane
ExxonMobil LD 503.LN Foams and Compounding Resin
J6 Polymers JFOAM™ A-204 Engineered Specialty Foam
J6 Polymers JFOAM™ FA-210 Engineered Specialty Foam

PLEND02 / 50777

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.